E 4318 Stainless Steels to SFA-5.1/SFA-5.1M

E 4318 - Specification & Application

  • SFA-5.1/SFA-5.1M - Carbon Steel Electrodes for Shielded Metal Arc Welding

Carbon Steel Electrodes for Shielded Metal Arc Welding

Chemical composition(wt.%) of E 4318 grade: to SFA-5.1/SFA-5.1M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Ni 13.00 15.00
Cr 17.00 19.00
Al - -
Cu - -
Ti - -
Fe - -
N - -
Mo 1.75 2.75
V - -

E 4318 - Detail

Carbon Steel Electrodes for Shielded Metal Arc Welding

Mechanical properties of grade E 4318 SFA-5.1/SFA-5.1M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
532 (≥) 181 (≥) 12 13 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 214

Physical properties of grade E 4318 SFA-5.1/SFA-5.1M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
411 (≥) 552 (≥) 23 41 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 422
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
595 257 599

Equivalent Products

We can customize the production of E 4318 grade, contact us for the best solution.
sales@specificsteel.com