ER 409Cb Stainless Steels to A5.9/A5.9M

ER 409Cb - Specification & Application

  • A5.9/A5.9M - Bare Stainless Steel Welding Electrodes and Rods

Bare Stainless Steel Welding Electrodes and Rods

Chemical composition(wt.%) of ER 409Cb grade: to A5.9/A5.9M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 1.00
Mn - 1.00
P - 0.045
S - 0.04
Ni - 0.50
Cr 10.50 11.75
Al - -
Cu - -
Ti - -
Fe - remaining
N - -
Mo - -
V - -

ER 409Cb - Detail

Bare Stainless Steel Welding Electrodes and Rods

Mechanical properties of grade ER 409Cb A5.9/A5.9M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
319 (≥) 583 (≥) 12 42 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade ER 409Cb A5.9/A5.9M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
931 (≥) 377 (≥) 24 23 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 214
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
533 228 828

Equivalent Products

We can customize the production of ER 409Cb grade, contact us for the best solution.