EV3 Stainless Steels

EV3 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of EV3 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.20 -
Si 1.00 -
Mn 1.30 -
Cr 21.0 -
Ni 11.5 -

EV3 - Detail

Steel for exhaust valves

Mechanical properties of grade EV3

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
428 (≥) 436 (≥) 24 24 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 333

Physical properties of grade EV3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
966 (≥) 462 (≥) 33 12 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 343
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
773 113 219

Equivalent Products

We can customize the production of EV3 grade, contact us for the best solution.