Steel for exhaust valves
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.20 | - | ||
Si | 0.50 | - | ||
Mn | 5.00 | - | ||
Cr | 21.0 | - | ||
Ni | 4.50 | - | ||
N | 0.30 | - |
Steel for exhaust valves
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
482 (≥) | 978 (≥) | 31 | 21 | 31 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 241 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
877 (≥) | 589 (≥) | 43 | 43 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 412 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
118 | 822 | 967 |
We can customize the production of EV7 grade, contact us for the best solution.