EV9 Stainless Steels

EV9 - Specification & Application

Steel for exhaust valves

Chemical composition(wt.%) of EV9 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.50
Si 0.30 0.80
Mn - 1.00
P - 0.045
S - 0.030
Cr 12.0 15.0
Ni 12.0 15.0
Mo 0.20 0.50
W 1.50 3.00

EV9 - Detail

Steel for exhaust valves

Mechanical properties of grade EV9

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
923 (≥) 672 (≥) 23 33 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade EV9

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
145 (≥) 652 (≥) 11 44 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 424
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
671 615 484

Equivalent Products

We can customize the production of EV9 grade, contact us for the best solution.