F 837 Class A1-50 S31603 Stainless Steels to F 837M (2002)

F 837 Class A1-50 S31603 - Specification & Application

  • F 837M (2002) - Standard Specification for Stainless Steel Socket Head Cap Screws (Metric)

Standard Specification for Stainless Steel Socket Head Cap Screws (Metric)

Chemical composition(wt.%) of F 837 Class A1-50 S31603 grade: to F 837M (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.035
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00
N - 0.10

F 837 Class A1-50 S31603 - Detail

Standard Specification for Stainless Steel Socket Head Cap Screws (Metric)

Mechanical properties of grade F 837 Class A1-50 S31603 F 837M (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
236 (≥) 918 (≥) 34 11 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 134

Physical properties of grade F 837 Class A1-50 S31603 F 837M (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
728 (≥) 697 (≥) 24 31 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
724 997 124

Equivalent Products

We can customize the production of F 837 Class A1-50 S31603 grade, contact us for the best solution.