H-46 Stainless Steels to SAE J 467 (1968)

H-46 - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Special Purpose Alloys ("Superalloys")

Chemical composition(wt.%) of H-46 grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.17
Si - 0.40
Mn - 0.65
Ni - 0.45
Cr - 12.00
Al - -
Cu - -
Ti - -
Fe - remaining
Mo - 0.65
Co - -
V - 0.30
N - 0.08
Nb - 0.40

H-46 - Detail

Special Purpose Alloys ("Superalloys")

Mechanical properties of grade H-46 SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
297 (≥) 865 (≥) 11 42 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade H-46 SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
942 (≥) 988 (≥) 31 44 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 141
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
779 167 364

Equivalent Grade

Equivalent Products

We can customize the production of H-46 grade, contact us for the best solution.
sales@specificsteel.com