H15470 Stainless Steels

H15470 - Specification & Application

Intake valve steel

Chemical composition(wt.%) of H15470 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.42 0.52
Si 0.15 0.30
Mn 1.25 1.75
P - 0.040
S - 0.05

H15470 - Detail

Intake valve steel

Mechanical properties of grade H15470

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
455 (≥) 431 (≥) 44 13 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 333

Physical properties of grade H15470

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
759 (≥) 885 (≥) 44 14 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
749 249 924

Equivalent Grade

Equivalent Products

We can customize the production of H15470 grade, contact us for the best solution.