H86450 Stainless Steels

H86450 - Specification & Application

Steel for intake valves

Chemical composition(wt.%) of H86450 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.42 0.49
Si 0.15 0.30
Mn 0.70 1.05
P - 0.035
S - 0.04
Cr 0.35 0.65
Ni 0.35 0.75
Mo 0.15 0.25

H86450 - Detail

Steel for intake valves

Mechanical properties of grade H86450

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
842 (≥) 224 (≥) 43 12 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 431

Physical properties of grade H86450

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
777 (≥) 198 (≥) 34 41 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 412
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
286 522 835

Equivalent Products

We can customize the production of H86450 grade, contact us for the best solution.