HR208 Stainless Steels to BS 2HR 208 (2009)

HR208 - Specification & Application

  • BS 2HR 208 (2009) - Specification for nickel-chromium-iron alloy plate, sheet and strip: annealed (nickel base, Cr 15.5, Fe 8)
  • BS HR 208 - Specification for nickel-chromium-iron alloy sheet, strip and plate: annealed (Nickel base, Cr 15.5, Fe 8)

Specification for nickel-chromium-iron alloy sheet, strip and plate: annealed (Nickel base, Cr 15.5, Fe 8)

Chemical composition(wt.%) of HR208 grade: to BS 2HR 208 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 0.50
Mn - 1.00
P - -
S - 0.015
Cr 14.00 17.00
Ni 72.00 -
Mo - -
Co - -
Ti - -
Fe 6.00 10.00
Cu - 0.50

HR208 - Detail

Specification for nickel-chromium-iron alloy sheet, strip and plate: annealed (Nickel base, Cr 15.5, Fe 8)

Mechanical properties of grade HR208 BS 2HR 208 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
865 (≥) 242 (≥) 42 43 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 412

Physical properties of grade HR208 BS 2HR 208 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
755 (≥) 866 (≥) 34 24 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
618 715 828

Equivalent Grade

Equivalent Products

We can customize the production of HR208 grade, contact us for the best solution.
sales@specificsteel.com