Specification for nickel-cobalt-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 14.8, Mo 5, Al 4.8, Ti 1.2)
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.12 | 0.17 | ||
Si | - | 1.00 | ||
Mn | - | 1.00 | ||
P | - | - | ||
S | - | 0.015 | ||
Cr | 14.00 | 15.70 | ||
Ni | - | remaining | ||
Mo | 4.50 | 5.50 | ||
Co | 18.00 | 22.00 | ||
Ti | 0.90 | 1.50 | ||
Fe | - | 1.00 | ||
Al | 4.50 | 4.90 | ||
Cu | - | 0.20 | ||
B | 0.0030 | 0.0100 | ||
Bi | - | 0.0001 | ||
Pb | - | 0.0015 | ||
Ag | - | 0.0005 | ||
Zr | - | 0.15 |
Specification for nickel-cobalt-chromium-molybdenum-aluminium-titanium heat-resisting alloy billets, bars, forgings and parts (nickel base, Co 20, Cr 14.8, Mo 5, Al 4.8, Ti 1.2)
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
468 (≥) | 672 (≥) | 34 | 41 | 21 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 413 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
814 (≥) | 166 (≥) | 31 | 21 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 143 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
383 | 364 | 496 |
We can customize the production of HR3 grade, contact us for the best solution.
–sales@specificsteel.com