HS 556 Stainless Steels to SAE AMS 5831C (2009)

HS 556 - Specification & Application

  • SAE AMS 5831C (2009) - Alloy, Corrosion and Heat-Resistant, Welding Wire 29Fe - 22Cr - 21Ni - 18.5Co - 3.2Mo - 2.8W - 0.78Ta 0.30Al - 0.05Zr - 0.05La - 0.20N

Alloy, Corrosion and Heat-Resistant, Welding Wire 29Fe - 22Cr - 21Ni - 18.5Co - 3.2Mo - 2.8W - 0.78Ta 0.30Al - 0.05Zr - 0.05La - 0.20N

Chemical composition(wt.%) of HS 556 grade: to SAE AMS 5831C (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.05 0.15
Si 0.20 0.80
Mn 0.50 2.00
Ni 19.00 22.50
Cr 21.00 23.00
Al 0.10 0.50
Cu - -
Ti - -
Fe - remaining
Mo 2.50 4.00
Co 16.00 21.00
W 2.00 3.50

HS 556 - Detail

Alloy, Corrosion and Heat-Resistant, Welding Wire 29Fe - 22Cr - 21Ni - 18.5Co - 3.2Mo - 2.8W - 0.78Ta 0.30Al - 0.05Zr - 0.05La - 0.20N

Mechanical properties of grade HS 556 SAE AMS 5831C (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
211 (≥) 787 (≥) 24 31 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade HS 556 SAE AMS 5831C (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
536 (≥) 235 (≥) 31 31 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 144
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
658 138 346