J 2613 Stainless Steels to SAE J 2613 (2009)

J 2613 - Specification & Application

  • SAE J 2613 (2009) - Welded Flash Controlled, High Strength (500 MPa Tensile Strength) Low Alloy Steel Hydraulic Tubing, Sub-Critically Annealed for Bending, Double Flaring, and Bending

Welded Flash Controlled, High Strength (500 MPa Tensile Strength) Low Alloy Steel Hydraulic Tubing, Sub-Critically Annealed for Bending, Double Flaring, and Bending

Chemical composition(wt.%) of J 2613 grade: to SAE J 2613 (2009)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.06
Si - 0.75
Mn - 0.75
P - -
S - -
Ni - 0.50
Cr 25.00 27.00
Al - -
Cu - 0.20
Ti - -
Fe - -
N - 0.04
Mo 0.75 1.50

J 2613 - Detail

Welded Flash Controlled, High Strength (500 MPa Tensile Strength) Low Alloy Steel Hydraulic Tubing, Sub-Critically Annealed for Bending, Double Flaring, and Bending

Mechanical properties of grade J 2613 SAE J 2613 (2009)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
825 (≥) 242 (≥) 43 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade J 2613 SAE J 2613 (2009)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
374 (≥) 629 (≥) 31 12 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
194 283 997

Equivalent Products

We can customize the production of J 2613 grade, contact us for the best solution.
sales@specificsteel.com