K12249 Stainless Steels

K12249 - Specification & Application

Alloy Steel

Chemical composition(wt.%) of K12249 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.60
Si - -
Mn 7.00 10.00
P - -
S - -
Ni 3.50 5.00
Cr - -
Al - -
Cu - -
Ti - -
Fe - -
N 0.30 0.50
Mo - -

K12249 - Detail

Alloy Steel

Mechanical properties of grade K12249

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
946 (≥) 513 (≥) 21 24 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 444

Physical properties of grade K12249

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
921 (≥) 237 (≥) 24 22 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 333
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
957 488 695

Equivalent Grade

Equivalent Products

We can customize the production of K12249 grade, contact us for the best solution.
sales@specificsteel.com