L-605 Stainless Steels to SAE J 467 (1968)

L-605 - Specification & Application

  • SAE J 467 (1968) - Special Purpose Alloys ("Superalloys")

Special Purpose Alloys ("Superalloys")

Chemical composition(wt.%) of L-605 grade: to SAE J 467 (1968)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.60
Mn - 1.50
Ni - 10.00
Cr - 20.00
Al - -
Cu - -
Ti - -
Fe - 1.60
Mo - -
Co - remaining
W - 15.00

L-605 - Detail

Special Purpose Alloys ("Superalloys")

Mechanical properties of grade L-605 SAE J 467 (1968)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
324 (≥) 989 (≥) 12 41 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 213

Physical properties of grade L-605 SAE J 467 (1968)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
993 (≥) 542 (≥) 22 24 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 121
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
471 626 816