MONEL K-500 Superalloys

MONEL K-500 - Specification & Application

Mainly used in the manufacture of aircraft engine working temperature in turbine blade and gas turbine blade below 750 DEG C; for fasteners

Chemical composition(wt.%) of MONEL K-500 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
Ni 63.00 -
C - 0.25
Mn - 1.50
Fe - 2.00
S - 0.01
Si - 0.50
Cu 27.00 33.00
Al 2.30 3.15
Ti 0.35 0.85

MONEL K-500 - Detail

Mainly used in the manufacture of aircraft engine working temperature in turbine blade and gas turbine blade below 750 DEG C; for fasteners, manufacturing ship spring; chemical equipment of the pump, valve parts; papermaking equipment on the scraping blade.

Mechanical properties of grade MONEL K-500

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
524 (≥) 726 (≥) 13 34 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 324

Physical properties of grade MONEL K-500

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
634 (≥) 393 (≥) 11 23 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 413
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
519 575 244

Equivalent Grade

Equivalent Products

We can customize the production of MONEL K-500 grade, contact us for the best solution.