NCF 601 Stainless Steels to G 4901 (2008)

NCF 601 - Specification & Application

  • G 4901 (2008) - Corrosion-resisting and heat-resisting superalloy bars

Corrosion-resisting and heat-resisting superalloy bars

Chemical composition(wt.%) of NCF 601 grade: to G 4901 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.10
Si - 0.50
Mn - 1.00
P - 0.03
S - 0.015
Cr 21.00 25.00
Ni 58.00 63.00
Cu - 1.00
Al 1.00 1.70
Ti - -
Fe remaining -

NCF 601 - Detail

Corrosion-resisting and heat-resisting superalloy bars

Mechanical properties of grade NCF 601 G 4901 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
412 (≥) 764 (≥) 23 11 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 111

Physical properties of grade NCF 601 G 4901 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
273 (≥) 374 (≥) 44 11 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 332
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
469 249 865

Equivalent Grade

Equivalent Products

We can customize the production of NCF 601 grade, contact us for the best solution.