NCF 690 TP Stainless Steels to G 4903 (2008)

NCF 690 TP - Specification & Application

  • G 4903 (2008) - Seamless nickel-chromium-iron alloy pipes

Seamless nickel-chromium-iron alloy pipes

Chemical composition(wt.%) of NCF 690 TP grade: to G 4903 (2008)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.50
Mn - 0.50
P - 0.03
S - 0.015
Cr 27.00 31.00
Ni 58.00 -
Cu - 0.50
Al - -
Ti - -
Fe - -

NCF 690 TP - Detail

Seamless nickel-chromium-iron alloy pipes

Mechanical properties of grade NCF 690 TP G 4903 (2008)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
532 (≥) 638 (≥) 22 41 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 242

Physical properties of grade NCF 690 TP G 4903 (2008)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
355 (≥) 576 (≥) 43 34 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 323
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
834 498 881