NCF825 Stainless Steels

NCF825 - Specification & Application

CNS Standard heat resistant alloy and corrosion resistant alloy bar and plate type and chemical composition

Chemical composition(wt.%) of NCF825 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 0.50
Mn - 1.00
P - 0.030
S - 0.015
Cr 19.00 23.00
Ni 38.00 46.00
Cu 1.50 3.50
Al - 0.20
Ti 0.60 1.20
Fe - remaining
Mo 2.50 3.50

NCF825 - Detail

CNS Standard heat resistant alloy and corrosion resistant alloy bar and plate type and chemical composition

Mechanical properties of grade NCF825

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
712 (≥) 929 (≥) 23 31 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 332

Physical properties of grade NCF825

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
515 (≥) 219 (≥) 33 24 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
938 642 674