NV3/NE8150 Stainless Steels

NV3/NE8150 - Specification & Application

Intake valve steel

Chemical composition(wt.%) of NV3/NE8150 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.50
Si - 0.30
Mn - 0.80
P -
S -
Ni - 0.30
Mo - 0.15

NV3/NE8150 - Detail

Intake valve steel

Mechanical properties of grade NV3/NE8150

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
154 (≥) 211 (≥) 34 14 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade NV3/NE8150

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
644 (≥) 533 (≥) 34 33 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 441
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
451 331 457

Equivalent Products

We can customize the production of NV3/NE8150 grade, contact us for the best solution.