Steel for intake valves
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | 0.39 | - | ||
Si | 0.25 | - | ||
Mn | 0.75 | - |
Steel for intake valves
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
383 (≥) | 741 (≥) | 41 | 42 | 14 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 232 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
567 (≥) | 418 (≥) | 44 | 42 | 42 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 331 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
274 | 142 | 634 |
We can customize the production of NV9 grade, contact us for the best solution.