Ni Span C902 Stainless Steels to SAE AMS 5223F (2002)

Ni Span C902 - Specification & Application

  • SAE AMS 5223F (2002) - Iron-Nickel Alloy, Strip, 49Fe - 5.3Cr - 42Ni - 2.5Ti - 0.55Al, Solution Heat Treated, Cold Rolled, 10% Reduction

Iron-Nickel Alloy, Strip, 49Fe - 5.3Cr - 42Ni - 2.5Ti - 0.55Al, Solution Heat Treated, Cold Rolled, 10% Reduction

Chemical composition(wt.%) of Ni Span C902 grade: to SAE AMS 5223F (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - -
Mn - -
Cr - 5.30
Ni - 42.50
Mo - -
Co - -
W - -
Al - 0.50
Cu - -
Ti - -
Fe - 49.00

Ni Span C902 - Detail

Iron-Nickel Alloy, Strip, 49Fe - 5.3Cr - 42Ni - 2.5Ti - 0.55Al, Solution Heat Treated, Cold Rolled, 10% Reduction

Mechanical properties of grade Ni Span C902 SAE AMS 5223F (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
594 (≥) 938 (≥) 31 22 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 321

Physical properties of grade Ni Span C902 SAE AMS 5223F (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
862 (≥) 137 (≥) 23 13 12 Solution and Aging, Annealing, Ausaging, Q+T,etc 234
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
926 613 496