Chemical composition(wt.%) of NiCr15Fe7TiAI grade: to NF EN 10269

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.50
Mn - 1.00
P - 0.020
S - 0.015
Cr 14.00 17.00
Ni 70.00 -
Mo - -
Ti 1.80 2.70
Co - 1.00
Al 0.40 1.00
Fe 5.00 9.00
Cu - 0.50
Nb+Ta 0.70 1.20

NiCr15Fe7TiAI - Detail

Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Mechanical properties of grade NiCr15Fe7TiAI NF EN 10269

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
412 (≥) 514 (≥) 21 31 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 421

Physical properties of grade NiCr15Fe7TiAI NF EN 10269

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
917 (≥) 836 (≥) 14 34 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 242
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
562 222 395