NiCr15Fe7TiAl Stainless Steels to ISO 683-15 (1992)

NiCr15Fe7TiAl - Specification & Application

  • ISO 683-15 (1992) - Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Chemical composition(wt.%) of NiCr15Fe7TiAl grade: to ISO 683-15 (1992)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.03 0.10
Si - 0.50
Mn - 0.50
P - 0.015
S - 0.015
Cr 14.00 17.00
Mo - 0.15
Ni remaining -
Al 1.10 1.35
Fe 5.00 9.00
Nb+Ta 0.70 1.20
Ti 2.00 2.60

NiCr15Fe7TiAl - Detail

Heat-treatable steels, alloy steels and free-cutting steels -- Part 15: Valve steels for internal combustion engines

Mechanical properties of grade NiCr15Fe7TiAl ISO 683-15 (1992)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
633 (≥) 111 (≥) 32 11 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 432

Physical properties of grade NiCr15Fe7TiAl ISO 683-15 (1992)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
793 (≥) 112 (≥) 33 34 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
942 695 868

Equivalent Products