Nonmagnetizable Steel
Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
---|---|---|---|---|
C | - | 0.55 | ||
Mn | - | 18 | ||
Cr | - | 4.5 |
X55MnCr18-5 X55MnCr18-4 18Mn-4Cr
Proof strength Rp0.2 (MPa) |
Tensile strength Rm (MPa) |
Impact energy KV (J) |
Elongation at fracture A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | Brinell hardness (HBW) |
---|---|---|---|---|---|---|
126 (≥) | 671 (≥) | 31 | 33 | 33 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 134 |
Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
Modulus of elasticity kN/mm2 |
Expansion rate |
---|---|---|---|---|---|---|---|
974 (≥) | 993 (≥) | 32 | 41 | 13 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 431 | |
Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
|||||
736 | 117 | 338 |
We can customize the production of Nonmagnetizable Steel X55MnCr18-5 / 18Mn-4Cr grade, contact us for the best solution.