S.152 Stainless Steels to BS S 152

S.152 - Specification & Application

  • BS S 152 - Specification for chromium-cobalt-molybdenum-vanadium-niobium heat-resisting steel billets, bars, forgings and parts (consumable electrode remelted) (1000-1140 MPa) (Cr 10.5, Co 6, Mo 0.8, V 0.2, Nb 0.3)

Specification for chromium-cobalt-molybdenum-vanadium-niobium heat-resisting steel billets, bars, forgings and parts (consumable electrode remelted) (1000-1140 MPa) (Cr 10.5, Co 6, Mo 0.8, V 0.2, Nb 0.3)

Chemical composition(wt.%) of S.152 grade: to BS S 152

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.06 0.11
Si 0.10 0.70
Mn 0.60 1.10
P - 0.028
S - 0.020
Cr 9.20 11.20
Ni 0.20 0.80
Mo 0.50 1.00
Nb 0.20 0.45
Co 5.00 7.00
V 0.10 0.35
N 0.010 0.035
B 0.004 0.012

S.152 - Detail

Specification for chromium-cobalt-molybdenum-vanadium-niobium heat-resisting steel billets, bars, forgings and parts (consumable electrode remelted) (1000-1140 MPa) (Cr 10.5, Co 6, Mo 0.8, V 0.2, Nb 0.3)

Mechanical properties of grade S.152 BS S 152

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
553 (≥) 377 (≥) 13 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 133

Physical properties of grade S.152 BS S 152

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
818 (≥) 182 (≥) 43 31 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
949 741 468

Equivalent Grade

Equivalent Products

We can customize the production of S.152 grade, contact us for the best solution.