S.527 Stainless Steels to BS S 527

S.527 - Specification & Application

  • BS S 527 - Specification for softened 18/10 chromium-nickel corrosion-resisting steel sheet and strip (niobium stabilized: 540 MPa)

Specification for softened 18/10 chromium-nickel corrosion-resisting steel sheet and strip (niobium stabilized: 540 MPa)

Chemical composition(wt.%) of S.527 grade: to BS S 527

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si 0.20 1.00
Mn 0.50 2.00
P - 0.035
S - 0.025
Cr 17.00 19.00
Ni 9.00 11.00
Mo - -
Nb 10×C 1.00

S.527 - Detail

Specification for softened 18/10 chromium-nickel corrosion-resisting steel sheet and strip (niobium stabilized: 540 MPa)

Mechanical properties of grade S.527 BS S 527

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
518 (≥) 157 (≥) 31 43 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade S.527 BS S 527

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
774 (≥) 226 (≥) 41 44 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
634 491 725

Equivalent Grade

Equivalent Products

We can customize the production of S.527 grade, contact us for the best solution.