S24100 Stainless Steels

S24100 - Specification & Application

S24100

Chemical composition(wt.%) of S24100 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 11.0 14.0
P - 0.045
S - 0.030
Si - 1.00
Ni 0.5 2.5
Cr 16.5 19.00
N 0.20 0.45

S24100 - Detail

S24100

Mechanical properties of grade S24100

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
632 (≥) 547 (≥) 23 22 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 333

Physical properties of grade S24100

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
335 (≥) 252 (≥) 22 22 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 142
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
998 652 921