S28200 Stainless Steels

S28200 - Specification & Application

Austenitic Chromium Manganese Copper Molybdenum Stainless Steel

Chemical composition(wt.%) of S28200 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn 17.00 19.00
Si - 1.00
P - 0.045
S - 0.03
Cr 17.50 19.50
Ni - -
Mo 0.50 1.50
N 0.40 0.60
Cu 0.50 1.50

S28200 - Detail

Austenitic Chromium Manganese Copper Molybdenum Stainless Steel

Mechanical properties of grade S28200

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
952 (≥) 269 (≥) 31 42 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade S28200

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
522 (≥) 132 (≥) 12 21 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 414
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
461 447 548

Equivalent Products

We can customize the production of S28200 grade, contact us for the best solution.
sales@specificsteel.com