S33228 Stainless Steels

S33228 - Specification & Application

Austenitic Nickel Chromium Heat Resisting Stainless Steel (Nicrofer 3228 NbCe)

Chemical composition(wt.%) of S33228 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Mn - 1.00
Si - 0.30
P - 0.02
S - 0.015
Cr 26.0 28.0
Ni 31.0 33.0
Ce 0.05 0.10
Nb 0.10 1.00
Al - 0.025

S33228 - Detail

Austenitic Nickel Chromium Heat Resisting Stainless Steel (Nicrofer 3228 NbCe)

Mechanical properties of grade S33228

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
897 (≥) 659 (≥) 11 21 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade S33228

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
148 (≥) 786 (≥) 43 31 34 Solution and Aging, Annealing, Ausaging, Q+T,etc 413
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
159 619 499

Equivalent Products

We can customize the production of S33228 grade, contact us for the best solution.