S37000 Stainless Steels

S37000 - Specification & Application

Austenitic Chromium Nickel Molybdenum Titanium Stainless Steel

Chemical composition(wt.%) of S37000 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.03 0.05
Mn 1.65 2.35
Si 0.50 1.00
P - 0.04
S - 0.01
Cr 12.50 14.50
Ni 14.50 16.50
Mo 1.50 2.50
N - 0.005
Ti 0.10 0.40
Co - 0.05

S37000 - Detail

Austenitic Chromium Nickel Molybdenum Titanium Stainless Steel

Mechanical properties of grade S37000

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
423 (≥) 623 (≥) 43 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade S37000

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
235 (≥) 287 (≥) 43 21 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
738 469 935

Equivalent Grade

Equivalent Products

We can customize the production of S37000 grade, contact us for the best solution.