S38100 Stainless Steels

S38100 - Specification & Application

Austenitic Chromium Nickel Silicon Stainless Steel

Chemical composition(wt.%) of S38100 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Mn - 2.00
Si 1.50 2.50
P - 0.03
S - 0.03
Cr 17.00 19.00
Ni 17.50 18.50
Mo - -

S38100 - Detail

Austenitic Chromium Nickel Silicon Stainless Steel

Mechanical properties of grade S38100

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
124 (≥) 393 (≥) 34 31 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 131

Physical properties of grade S38100

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
345 (≥) 725 (≥) 11 14 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 113
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
844 478 666