S41001 Stainless Steels

S41001 - Specification & Application

Chromium Super Strength Steel

Chemical composition(wt.%) of S41001 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Mn - 1.00
Si - 1.00
P - 0.025
S - 0.025
Cr 11.50 13.50
Ni - 0.75
Mo - 0.50
Al - 0.05
Cu - 0.05
Sn - 0.05

S41001 - Detail

Chromium Super Strength Steel

Mechanical properties of grade S41001

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
195 (≥) 818 (≥) 24 42 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 144

Physical properties of grade S41001

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
396 (≥) 658 (≥) 32 22 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
295 781 349

Equivalent Grade

Equivalent Products

We can customize the production of S41001 grade, contact us for the best solution.
sales@specificsteel.com