S41880 Stainless Steels

S41880 - Specification & Application

Martensitic Chromium Wolfram Nickel Stainless and Heat Resisting Steel Bare Filler Metal (Greek Ascoloy)

Chemical composition(wt.%) of S41880 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.20
Si - 0.50
Mn - 1.00
P - -
S - -
Ni - -
Cr - 12.50
Al - -
Cu - -
Ti - -
Fe - remaining
N - -
Mo - -
W - 3.00

S41880 - Detail

Martensitic Chromium Wolfram Nickel Stainless and Heat Resisting Steel Bare Filler Metal (Greek Ascoloy)

Mechanical properties of grade S41880

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
245 (≥) 198 (≥) 13 23 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade S41880

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
319 (≥) 848 (≥) 33 41 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 233
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
197 232 283

Equivalent Products

We can customize the production of S41880 grade, contact us for the best solution.
sales@specificsteel.com