SA-213 TP347LN Stainless Steels to SA-213/SA-213M

SA-213 TP347LN - Specification & Application

  • SA-213/SA-213M - Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Chemical composition(wt.%) of SA-213 TP347LN grade: to SA-213/SA-213M

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.005 0.02
Si - 0.75
Mn - 2.00
P - 0.04
S - 0.03
Ni 9.00 13.00
Cr 17.00 20.00
Al - -
Cu - -
Ti - -
Fe - -
N 0.06 0.10
Mo - -
V - -

SA-213 TP347LN - Detail

Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes

Mechanical properties of grade SA-213 TP347LN SA-213/SA-213M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
248 (≥) 318 (≥) 34 34 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 344

Physical properties of grade SA-213 TP347LN SA-213/SA-213M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
233 (≥) 188 (≥) 11 33 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 213
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
826 288 787

Equivalent Products