SA-249 S31725 Stainless Steels to SA-249/SA-249M

SA-249 S31725 - Specification & Application

  • SA-249/SA-249M - Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Chemical composition(wt.%) of SA-249 S31725 grade: to SA-249/SA-249M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Mn - 2.00
Si - 1.00
P - 0.045
S - 0.03
Cr 18.00 20.00
Ni 13.50 17.50
Mo 4.00 5.00
N - 0.10

SA-249 S31725 - Detail

Specification for Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes

Mechanical properties of grade SA-249 S31725 SA-249/SA-249M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
473 (≥) 212 (≥) 11 21 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 443

Physical properties of grade SA-249 S31725 SA-249/SA-249M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
591 (≥) 394 (≥) 31 11 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 134
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
311 795 825