SA-312 S33228 Stainless Steels to SA-312/SA-312M

SA-312 S33228 - Specification & Application

  • SA-312/SA-312M - Specification for Seamless and Welded Austenitic Stainless Steel Pipes

Specification for Seamless and Welded Austenitic Stainless Steel Pipes

Chemical composition(wt.%) of SA-312 S33228 grade: to SA-312/SA-312M

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.04 0.08
Mn - 1.00
Si - 0.30
P - 0.02
S - 0.015
Cr 26.0 28.0
Ni 31.0 33.0
Ce 0.05 0.10
Nb 0.10 1.00
Al - 0.025

SA-312 S33228 - Detail

Specification for Seamless and Welded Austenitic Stainless Steel Pipes

Mechanical properties of grade SA-312 S33228 SA-312/SA-312M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
497 (≥) 184 (≥) 21 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 124

Physical properties of grade SA-312 S33228 SA-312/SA-312M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
322 (≥) 385 (≥) 43 23 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 442
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
257 287 942

Equivalent Products

We can customize the production of SA-312 S33228 grade, contact us for the best solution.