SA-803 29-4-2 Stainless Steels to SA-803/SA-803M

SA-803 29-4-2 - Specification & Application

  • SA-803/SA-803M - Specification for Welded Ferritic Stainless Steel Feedwater Heater Tubes

Specification for Welded Ferritic Stainless Steel Feedwater Heater Tubes

Chemical composition(wt.%) of SA-803 29-4-2 grade: to SA-803/SA-803M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.01
Si - 0.20
Mn - 0.30
P - -
S - -
Ni 2.00 2.50
Cr 28.00 30.00
Al - -
Cu - 0.15
Ti - -
Fe - -
N - 0.02
Mo 3.50 4.20

SA-803 29-4-2 - Detail

Specification for Welded Ferritic Stainless Steel Feedwater Heater Tubes

Mechanical properties of grade SA-803 29-4-2 SA-803/SA-803M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
154 (≥) 349 (≥) 12 32 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 224

Physical properties of grade SA-803 29-4-2 SA-803/SA-803M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
558 (≥) 416 (≥) 13 44 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 141
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
772 311 252

Equivalent Products

We can customize the production of SA-803 29-4-2 grade, contact us for the best solution.