SA-965 Grade F316LN Stainless Steels to SA-965/SA-965M

SA-965 Grade F316LN - Specification & Application

  • SA-965/SA-965M - Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts

Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts

Chemical composition(wt.%) of SA-965 Grade F316LN grade: to SA-965/SA-965M

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 0.75
Mn - 2.00
P - 0.045
S - 0.035
Cr 16.0 18.0
Ni 10.0 14.0
Mo 2.00 3.00
N 0.10 0.16

SA-965 Grade F316LN - Detail

Specification for Steel Forgings, Austenitic, for Pressure and High Temperature Parts

Mechanical properties of grade SA-965 Grade F316LN SA-965/SA-965M

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
272 (≥) 161 (≥) 32 13 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade SA-965 Grade F316LN SA-965/SA-965M

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
977 (≥) 561 (≥) 14 43 21 Solution and Aging, Annealing, Ausaging, Q+T,etc 334
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
146 332 291

Equivalent Products

We can customize the production of SA-965 Grade F316LN grade, contact us for the best solution.