STS304N1 Stainless Steels to D 3535 (2002)

STS304N1 - Specification & Application

  • D 3535 (2002) - Stainless steel wires for springs
  • D 3698 (2008) - Cold rolled stainless steel plates, sheets and strip
  • D 3702 (2008) - Stainless steel wire rods
  • D 3703 (2007) - Stainless steel wires
  • D 3705 (2008) - Hot rolled stainless steel plates, sheets and strip
  • D 3706 (2008) - Stainless steel bars

Stainless steel bars

Chemical composition(wt.%) of STS304N1 grade: to D 3535 (2002)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.50
P - 0.045
S - 0.030
Cr 18.00 20.00
Ni 7.00 10.50
Mo - -
N 0.10 0.25

STS304N1 - Detail

Stainless steel bars

Mechanical properties of grade STS304N1 D 3535 (2002)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
299 (≥) 447 (≥) 14 42 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 141

Physical properties of grade STS304N1 D 3535 (2002)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
925 (≥) 586 (≥) 22 11 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
319 525 677