SUH 310 Stainless Steels to G 4312 (2011)

SUH 310 - Specification & Application

  • G 4312 (2011) - Heat-resisting steel plate, sheet and strip

Heat-resisting steel plate, sheet and strip

Chemical composition(wt.%) of SUH 310 grade: to G 4312 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.45
Si 1.50 2.50
Mn - 0.60
P - 0.04
S - 0.03
Cr 14.00 16.00
Ni 13.00 15.00
Mo - -
W 2.00 3.00

SUH 310 - Detail

Heat-resisting steel plate, sheet and strip

Mechanical properties of grade SUH 310 G 4312 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
744 (≥) 583 (≥) 14 12 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 314

Physical properties of grade SUH 310 G 4312 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
714 (≥) 162 (≥) 34 23 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 343
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
582 448 265

Equivalent Products

We can customize the production of SUH 310 grade, contact us for the best solution.