SUH 38 Stainless Steels to G 4311 (2011)

SUH 38 - Specification & Application

  • G 4311 (2011) - Heat-resisting steel bars and wire rods

Heat-resisting steel bars and wire rods

Chemical composition(wt.%) of SUH 38 grade: to G 4311 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.25 0.35
Si - 1.00
Mn - 1.20
P 0.18 0.25
S - 0.03
Cr 19.00 21.00
Ni 10.00 12.00
Mo 1.80 2.50
B 0.001 0.010

SUH 38 - Detail

Heat-resisting steel bars and wire rods

Mechanical properties of grade SUH 38 G 4311 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
476 (≥) 986 (≥) 34 44 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 422

Physical properties of grade SUH 38 G 4311 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
834 (≥) 255 (≥) 43 32 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 124
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
944 373 789

Equivalent Grade

Equivalent Products

We can customize the production of SUH 38 grade, contact us for the best solution.
sales@specificsteel.com