SUH660 Stainless Steels to G 4312 (2011)

SUH660 - Specification & Application

  • G 4312 (2011) - Heat-resisting steel plate, sheet and strip

Heat-resisting steel plate, sheet and strip

Chemical composition(wt.%) of SUH660 grade: to G 4312 (2011)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.04
S - 0.03
Cr 13.50 16.00
Ni 24.00 27.00
Mo 1.00 1.50
Ti 1.90 2.35
V 0.10 0.50
Al - 0.35
B 0.001 0.010

SUH660 - Detail

Heat-resisting steel plate, sheet and strip

Mechanical properties of grade SUH660 G 4312 (2011)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
478 (≥) 339 (≥) 34 42 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 433

Physical properties of grade SUH660 G 4312 (2011)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
186 (≥) 576 (≥) 23 23 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 123
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
521 721 998

Equivalent Products

We can customize the production of SUH660 grade, contact us for the best solution.