SUS 303Se Stainless Steels to G 4303 (2005)

SUS 303Se - Specification & Application

  • G 4303 (2005) - Stainless steel bars
  • G 4308 (2007) - Stainless steel wire rods
  • G 4309 (1999) - Stainless steel wires
  • G 4318 (2007) - Cold finished stainless steel bars

Standard Specification for Stainless Steel Socket Set Screws (Metric)

Chemical composition(wt.%) of SUS 303Se grade: to G 4303 (2005)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 2.00
P - 0.2
S - 0.06
Cr 17.0 19.0
Ni 8.00 10.0
Se 0.15 -

SUS 303Se - Detail

Austenitic Alloys; Sizes M1.6 through M24
Standard Specification for Stainless Steel Socket Set Screws (Metric)

Mechanical properties of grade SUS 303Se G 4303 (2005)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
538 (≥) 353 (≥) 21 14 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 211

Physical properties of grade SUS 303Se G 4303 (2005)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
215 (≥) 853 (≥) 14 32 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 131
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
827 813 772

Equivalent Products

We can customize the production of SUS 303Se grade, contact us for the best solution.