SUS 316 J1 L Stainless Steels to G 4303 (2012)

SUS 316 J1 L - Specification & Application

  • G 4303 (2012) - Stainless steel bars

Stainless steel bars

Chemical composition(wt.%) of SUS 316 J1 L grade: to G 4303 (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 17.00 19.00
Ni 12.00 16.00
Mo 1.20 2.75
N - -
Cu 1.00 2.50

SUS 316 J1 L - Detail

Stainless steel bars

Mechanical properties of grade SUS 316 J1 L G 4303 (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
652 (≥) 756 (≥) 14 43 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade SUS 316 J1 L G 4303 (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
299 (≥) 291 (≥) 42 33 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 344
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
815 185 215