Chemical composition(wt.%) of SUS 316A grade: to G 4321 (2000)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 1.00
Mn - 2.00
P - 0.045
S - 0.03
Cr 16.00 18.00
Ni 10.00 14.00
N - -
Mo 2.00 3.00

SUS 316A - Detail

Stainless steel for building structure

Mechanical properties of grade SUS 316A G 4321 (2000)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
869 (≥) 152 (≥) 41 14 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 121

Physical properties of grade SUS 316A G 4321 (2000)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
983 (≥) 827 (≥) 31 14 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 114
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
475 892 889