SUS 436L Stainless Steels to G 4305 (2012)

SUS 436L - Specification & Application

  • G 4305 (2012) - Cold-rolled stainless steel plate, sheet and strip

Cold-rolled stainless steel plate, sheet and strip

Chemical composition(wt.%) of SUS 436L grade: to G 4305 (2012)

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.025
Si - 1.00
Mn - 1.00
P - 0.04
S - 0.03
Cr 16.00 19.00
Ni - 0.60
Mo 0.75 1.50
N - 0.025

SUS 436L - Detail

Cold-rolled stainless steel plate, sheet and strip

Mechanical properties of grade SUS 436L G 4305 (2012)

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
121 (≥) 384 (≥) 13 14 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 331

Physical properties of grade SUS 436L G 4305 (2012)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
115 (≥) 147 (≥) 44 11 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 322
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
738 452 479

Equivalent Products

We can customize the production of SUS 436L grade, contact us for the best solution.
sales@specificsteel.com