SUS303Se Stainless Steels to SA/JIS G4303

SUS303Se - Specification & Application

  • SA/JIS G4303 - Specification for stainless steel bars

Standard Specification for Stainless Steel Socket Set Screws (Metric)

Chemical composition(wt.%) of SUS303Se grade: to SA/JIS G4303

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.15
Si - 1.00
Mn - 2.00
P - 0.2
S - 0.06
Cr 17.0 19.0
Ni 8.00 10.0
Se 0.15 -

SUS303Se - Detail

Specification for stainless steel bars

Mechanical properties of grade SUS303Se SA/JIS G4303

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
258 (≥) 714 (≥) 41 22 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade SUS303Se SA/JIS G4303

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
918 (≥) 337 (≥) 14 14 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 341
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
731 248 891

Equivalent Products

We can customize the production of SUS303Se grade, contact us for the best solution.
sales@specificsteel.com