T2 Tool Die Steels

T2 - Specification & Application

High-Speed Tool Steel

Chemical composition(wt.%) of T2 grade:

Elements Min.(≥) Max.(≤) Similar Remarks
C 0.80 0.90
Si 0.20 0.40
Mn 0.20 0.40
P - 0.030
S - 0.030
Cr 3.75 4.50
Mo - 1.00
V 1.80 2.40
W 17.50 19.00
Co - -

T2 - Detail

High-Speed Tool Steel

Mechanical properties of grade T2

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
523 (≥) 691 (≥) 21 23 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade T2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
846 (≥) 378 (≥) 21 21 22 Solution and Aging, Annealing, Ausaging, Q+T,etc 423
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
937 945 969

Equivalent Products

We can customize the production of T2 grade, contact us for the best solution.
sales@specificsteel.com