X2CrMoTiS18-2 Stainless Steels to BS EN 10088-1

X2CrMoTiS18-2 - Specification & Application

  • BS EN 10088-1 - Stainless steels - Part 1: List of stainless steels
  • BS EN 10088-3 - Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
  • BS EN 10088-5 - Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes

Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes

Chemical composition(wt.%) of X2CrMoTiS18-2 grade: to BS EN 10088-1

Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.03
Si - 1.00
Mn - 0.50
P - 0.04
S 0.15 0.35
Cr 17.50 19.00
Ni - -
Mo 2.00 2.50
Ti 0.30 0.80
C+N - 0.040

X2CrMoTiS18-2 - Detail

Stainless steels - Part 5: Technical delivery conditions for bars, rods, wire, sections and bright products of corrosion resisting steels for construction purposes

Mechanical properties of grade X2CrMoTiS18-2 BS EN 10088-1

Proof strength
Rp0.2 (MPa)
Tensile strength
Rm (MPa)
Impact energy
KV (J)
Elongation at fracture
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition Brinell hardness (HBW)
742 (≥) 368 (≥) 12 42 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 231

Physical properties of grade X2CrMoTiS18-2 BS EN 10088-1

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
Modulus of elasticity
kN/mm2
Expansion rate
496 (≥) 118 (≥) 41 12 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 313
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
277 721 695

Equivalent Grade

Equivalent Products

We can customize the production of X2CrMoTiS18-2 grade, contact us for the best solution.